Re: [MW:12796] Differences between semi and fully killed steel

Si content shall be minimum 0.1 % or Al shall be minium 0.03% in case of fully killed steel verified by TC


 
On Sat, Oct 29, 2011 at 5:14 PM, meisam shokri arfaei <meisamshokri@gmail.com> wrote:
Dear experts,
I have a steel which marked as A516 Gr.70. I checked the metallugraphic structure and the microstructure is same as both semi and fully killed steel. (In SA516 it is defined that the quality grade shall be fully killed).
Now my question is:
 
How can I find that this steel is fully killed or semi killed?
Can anyone introduce any reference standard or handbook to differs between these two quality grades and also a test procedure for that purpose?
 
Regards

--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66283696
Fax: +98-21-66283693

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...