Re: [MW:12718] Backing Weld

Hi,

No, production welding with double sided weld joints can be carried out with PQR qualified for single sided weld joints, joint preparation is not an essential variable for procedure qualification, 

What thickness of pipe? if thickness is large or pipe is welded longitudinally the weld is strengthened by both side to achieve a joint factor of 1.

Client owe an answer to you for rejecting this practice, also please find below recommendation:-

"For double welded joints, the backside of joints shall be cleaned/gauged to sound metal unless it can be demonstrated that an acceptable weld can be made without this operation"

Regards
Manpreet Singh
Do Nothing Simply When a Way Can be Found to Make it Complex and Wonderful



From: Azam Mohd <azam1976@gmail.com>
Sent: Tue, 18 Oct 2011 19:33:06
To: materials-welding@googlegroups.com
Subject: [MW:12687] Backing Weld

Dear Experts,

Please share your experience

PQR is qualified for GTAW+SMAW Process for P1 material but because of ovality problem in the pipe it is required sometime to go for backing weld with GTAW process.

What will be the effect of backing weld on mechanical and chemical properties?

Client is not allowing for the backing weld. Is it necessary that PQR is to be qualified with backing weld?

If code is supporting for the Backing weld if PQR is not qualified for backing weld please send the reference for the same.

 

Thanks & Regards,

Azam

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...