Yes sand blasting and copper slag BLASTING HAS BEEN BANNED . BUT STILL THEY ARE
USING MOSTLY IN GULF COUNTRIES BCOZ THEY HAVE MORE SAND OF BLASTING FREE OF
COST OF COURSE IT IS FREE . COPPER SLAG TOO BANNED BUT STILL IN INDIA AND OTHER
COUNTRIES STILL USING. BEST SAFE IS GARNET BLAST. IT IS SAFE YES TILL ANY
ALTERNATE BLASTING MATERIALS COMES.


On Tue, 25 Oct 2011 14:19:42 +0530 wrote
>


v:* {
BEHAVIOR: url (#default#vml)
}


























Silica means the sand,.due to blasting,size of thesand would become very minute
and it will cause silicosys (lung desease)tothe human who is breathing the
same..

So internationaly sand blasting has been banned...

However copper slag can be used for abrasive blasting..






-------Original Message-------


From: Sreejith.Nair
Date: 9/22/2010 6:52:13 PM
To: materials-welding@googlegroups.com
Subject: [MW:7145] Copper Slag Abrasive
Hi everyone,
> I came across many coating specs which are having one common sentence "
Silica sand and copper slag shall not be used for blasting".
>
>What is the issue with using copper slag ? What are the dis advantages of
copper slag?
>--
>- Sreejith Nair-
>
>
--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding-
unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>










--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-
welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-
welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.
>


Dear Sir,





Thanking You,

Honesty is the best Policy

With Warm Regards,

Muthu Barathi P
Mobile No:00962788269821 (Jordan)
00962775401951

Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...