Dear All,
can anybody help :
we have some some small bore (1/2" ~ 1 1/2") gate valve in stock, when we open the valve by hand wheel and wedge goes up, some water comes out from inside of valve:
now my questions :
1-what is this water i n valve?
2-is it related to Hydro test?
3-can we reject these valves?
your prompt reply would be highly appreciated.
Regards,
Zarei
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
can anybody help :
we have some some small bore (1/2" ~ 1 1/2") gate valve in stock, when we open the valve by hand wheel and wedge goes up, some water comes out from inside of valve:
now my questions :
1-what is this water i n valve?
2-is it related to Hydro test?
3-can we reject these valves?
your prompt reply would be highly appreciated.
Regards,
Zarei
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments