Dear Pankaj,
Any NDT related work shall have a written procedure. These procedures may be in accordance with one or more codes or standards which support the user for some special works. In those procedures special situation for the work shall be defined. the first place that you have to search for such information about overlap of films is in written procedures.
But in general, there is a qualified range of film density that the interpreter can evaluate radiographic film in this range. The overlap shall be in such a way that each part of the film that is out of this range (usually lesser in density) repeats in next shoot within the in-range film density.
 
Regards

On Thu, Oct 20, 2011 at 10:38 PM, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:
Dear Pankaj,

Film overlap is given only for identification purpose that the same weld is continued.

Dont measure the density on the overlapped lighter area. Measure the density on un overlapped area of the previous film.

Its a general knowledge and no code says anything about that, as far as I know.

Nandeesh



--- On Thu, 20/10/11, pankaj.kolhe15 <pankaj.kolhe15@gmail.com> wrote:

From: pankaj.kolhe15 <pankaj.kolhe15@gmail.com>
Subject: [MW:12728] RT density
To: "pgoswami" <pgoswami@quickclic.net>, "materials-welding" <materials-welding@googlegroups.com>
Date: Thursday, 20 October, 2011, 3:09 PM


Dear sir,
what is the density requirement at overlapped area , if the two films
got overlapped
for gamma rays and where it is written

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66283696
Fax: +98-21-66283693

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...