Friday, October 28, 2011

Re: [MW:12787] quenching of stainless steel AISI304L

Dear Feyzullayev



It is impossible to quench the stainless steel 304. Because it is already a austenitic steel and what quenching ever you do it will be still austenitic so there will be no increasing in hardness





2011/10/27 Elshan Feyzullayev <elshan_f@hotmail.com>
Is it possible to quench the subjected steel?
 
best regards,
El.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Tuğrulhan ÖZDEMİR

Metalürji & Malzeme Müh. (Y.T.U.)

U.Kaynak Mühendisi (I.W.E.)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...