Sunday, October 23, 2011

Re: [MW:12758] P91 - Welder qualification

Hi,

Please review QW-350 (welder qualification), change is P no. would require requalification regardless of welding process.

Regards
Manpreet Singh



From: "Vinod Kataria" <vinod.kataria@blissanand.com>
Sent: Sat, 22 Oct 2011 16:38:25
To: <materials-welding@googlegroups.com>
Subject: Re: [MW:12735] P91 - Welder qualification

Dear All,

We have qualified procedure for Inconel 8825 P No. 45 as per ASME Section-9 with GTAW process using filler ErNiCrMo3, now we need to weld Inconel 625 P No. 43 with GTAW using the same filler i.e. ErNiCrMo3. Please suggest if we can use already qualified procedure for Inconel 825 for Inconel 625 also or we need to do the fresh qualification for this.

Thanks in advance for your kind help.

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...