Re: [MW:12776] what filler metal can weld 1.4825

Dear Roy,
 
Please provide the more details about materials (stad, code, compositions) and applications.
 
Regards
Amit Pahuja

On Tue, Oct 25, 2011 at 9:11 PM, Roy LIU刘艺 <standardliu@hotmail.com> wrote:
Hi, experts,

A furnace equipment wants to weld material 1.4825 (Material No.), which filler metals could be applied for this?


 

Best regards

 

Roy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...