The mfg TC must show fully killed to comformed the requirement.
 
There are also mfg TC available in market, in which Fully killed / killed is not mentioned, these kind of TCs should not be allowed to use if the requirement is Fully killed.

On Tue, Oct 18, 2011 at 9:45 AM, Vivek Joshi <hifromvivek@gmail.com> wrote:
Hello everybody,
Can somebody tell me please whether ASTM A106 Grade B is fully killed
steel by ASTM specification itself. If not then is it also avalable in
the form of Semi-Killed steel.
Vivek

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...