RE: [MW:12735] P91 - Welder qualification

Dear All,

We have qualified procedure for Inconel 8825 P No. 45 as per ASME Section-9 with GTAW process using filler ErNiCrMo3, now we need to weld Inconel 625 P No. 43 with GTAW using the same filler i.e. ErNiCrMo3. Please suggest if we can use already qualified procedure for Inconel 825 for Inconel 625 also or we need to do the fresh qualification for this.

Thanks in advance for your kind help.

With kind regards,

Vinod Kumar Kataria

GM - Operations

Bliss Anand Private Limited,

92B/93B Sector 5

IMT Manesar,Gurgaon,

National Capital Region Delhi.

India .

Phone : +91-124-4366000 (9 Lines)

Mobile Phone : +91-9560199004

Fax : +91-124-2290884