[MW:12761] Disimillar thickness & dissimilar garde material

Dear All Friends,

I want to make one Structural wps with material grade-
BSEN toASTM stnadard.
Material Thickness of BSEN Standard material is 19mm( CS)
And ASTM material is -3mm.(S.S)
Kindly give me some advice to how to make wps, which code
I have to follow, SEC-IX or BSEN-15614-1
How can I qualify the material thickness, If I will follow
ASME( its range only 0.5t to 2t ) then Multi PQR, how to do? & If I
follow
BSEN ( its range 0.5t to1.2T)how to do?

Thanks & Regards

Madhusudan Rout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...