AISI 8630H
Category Steel
Class  Alloy steel
Type  H-steel
Common Names Nickel-chromium-molybdenum steel
Designations  Germany: DIN 1.6545 
Italy: UNI 30 NiCrMo 2 KB 
United States: ASTM A304 , SAE J1268 , UNS H86300

http://www.efunda.com/materials/alloys/alloy_steels/show_alloy.cfm?ID=AISI_8630H&show_prop=all&Page_Title=AISI%208630H
On Fri, Jul 22, 2011 at 3:20 PM, V B <vikas.bhandari349@gmail.com> wrote:
Hi

I am not able to find mechanical properties/other details/equivalent of AISI 86 30H.I was wondering if  any of the member could throw some light in this regard. All I know is it is to be used as an end fitting for a riser.

Thanks 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...