Re: [MW:11841] Where we can find Impact testing recorded values @ - 34 C for SA 537 CL 1 Material

Dear suresh
 
Plz check the Code API 620 & 650 ..
 
Regards
 
A.J.Khan


--- On Wed, 20/7/11, Suresh <bobsuresh24@gmail.com> wrote:

From: Suresh <bobsuresh24@gmail.com>
Subject: [MW:11838] Where we can find Impact testing recorded values @ - 34 C for SA 537 CL 1 Material
To: materials-welding@googlegroups.com
Date: Wednesday, 20 July, 2011, 8:26 PM

Dear All ,
 
I would like to requesting you that ....We are doing Ammonia Tank erection which is using SA 537 CL 1 material ...
 
Now we are doing PQR for 537 Material @ - 34 C (which has tested by manufacturer ) and as per MDMT .
 
My Question is that here we can find the Impact recorded values for SA 537 CL1 @ - 34 C ...I need which code it was showing ...Client need that copy prior to go for PQR .
 
--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...