Dear Martin,
my answer :
1. Yes
2. No

Regards
Rudi

2011/7/9 Martin Prad <martin_prad@hotmail.com>
Gents,
 
Can we clear 2 questions here please?
 
1. To qualify the welders to 6GR position as per AWS D1.1 is it mandatory to have a WPS specific for 6GR position?
2. Is it possible using a WPS qualified for 6G position we can test the welders to 6GR? 
 
 
Thanks
Martin.  
 
 
 
 
> Date: Fri, 8 Jul 2011 04:12:03 -0700
> Subject: [MW:11633] Re: 6GR position
> From: fred.schweighardt@airliquide.com
> To: materials-welding@googlegroups.com

>
> Figure 4.13 in AWS D1.1:2010 shows an optional machining procedure for
> 6GR side bends
>
> On Jul 7, 7:47 am, Martin Prad <martin_p...@hotmail.com> wrote:
> > Hi experts,
> >
> > I would like to clear a point regarding the welder qualification in 6GR position. When the welder qualification test is carried out in 6GR position the ID of the pipe (6"x16mm is welded to 6"x22 mm with plate restriction as per Fig. 4.27 AWS D1.1) is offset. When the test pieces are prepared for bend test is it required to skim the root (offset) section by removing the offset or left as welded and carry out the bend test?
> >
> > Kind regards,
> > Martin.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...