Your distance depends if you want an actual 2 mR/hr boundary or a calculated one, What are they shooting,etc.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of limesh M
Sent: Monday, July 18, 2011 10:47 PM
To: Materials & Welding
Subject: [MW:11816] Ir92 with 32 Curie-What is the safe distance?

 

Dear All,

In one fabrication yard,IR192(Iridium192) Isotope being used to take radiography of welded joints to ensure it's integrity after visual inspection.NDT crew usually brings radiation source with a strength of 32 Curie(NDT contractor claiming that they are using 32 curie only but I don't know the exact strength.This is due to client pressure otherwise they are ready to bang with higher curies!!).I would like to know what would be the safe distance when IR92 with 32 curie strength operates without collimator.How can I calculate the safe distance from above parameters?I need this calculation urgently due to non availability of completely covered (except roof) concrete bunker or natural sand wall.For NDT crew protection during RT, two pieces of concrete wall provided to cover their body.Moreover, people like skilled/unskilled workers are staying very close(20Mtr to 35 Mtr range) to radiography area and nobody aware of the seriousness of the activity including the world famous client!!!

It will be highly appreciated if someone could provide an excel spread sheet to calculate the safe distance for different source strength.

Thanks in advance



Regards,


Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...