Hi Rinshad,
 
The details as follows,
 
Base Metal : S355J2/EH36
SMAW
Filler dia : 2.4 mm
DNV C401/ASME SEC IX
Iron content : Max 5%,
no PWHT


 
On Mon, Jul 18, 2011 at 9:38 PM, rinshad abdul rahman <rinshad043@gmail.com> wrote:
Dear Mr.Babu,
 
What is the process? ,filler dia ?,what are the test requirement ? ,which code your following ? ,give more details about your requirement
 
 
Regards
 
Rinshad

On Mon, Jul 18, 2011 at 3:27 PM, K.Babu <kbabupsg@gmail.com> wrote:
Gents,
 
I would like to some suggestions, on inconel overlay on S355J2 without PWHT
 
What are the steps to taken to reduce the iron content less than 5 %
 
Thanks & regards,

K.Babu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...