Nanesh already picked it, In additon, For PQR qualification ASME sec ix do not compell to perform any volumetric examination such as UT/RT but for welder qualification either UT or RT is required (2010 edition).
 
 Lack of Side wall fusion is perdominate defect generally found in GMAW/FCAW short circuit transfer hence UT examination is recommended for these process (API 577, welding inspection and metallurgy)
 
LOF problems can be solved by proper heat input and vertical uphill method.
 
Regards
Manpreet Singh


From: "Nandesh Kumar"nandeshkumar@rocketmail.com
Sent: Sun, 17 Jul 2011 22:56:45 +0530
To: materials-welding@googlegroups.com
Subject: Re: [MW:11759] PQR testing with RT & UT

Abhishek,
>
>Since, FCAW is more susceptible to lack of side wall fusion, RT may not detect such a defect and hence UT is the best suited method of NDT to detect LOF.
>
>Nandeesh
>
>
>--- On Fri, 15/7/11, ABHISHEK GHOSH <ghoshabhishekmech@gmail.com> wrote:
>

>From: ABHISHEK GHOSH <ghoshabhishekmech@gmail.com>
>Subject: [MW:11740] PQR testing with RT & UT
>To: materials-welding@googlegroups.com
>Date: Friday, 15 July, 2011, 3:57 PM
>
>
Dear Experts,

>
Why UT along with RT is performed while qualifying a procedure with FCAW welding, At which clause in ASME 9 it is mentioned that UT & RT both has to be performed ??

>
With regards.

>
AG

>--
>
ABHISHEK GHOSH
>FAHAHEEL, KUWAIT
>MOB: (00)965-65772043

>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...