Sunday, July 17, 2011

Re: [MW:11787] Inconel Filler metal / Welder's qualification

It is better to do pre production test for welders because inconel welding is not that easy like ss
pandithan

On Tue, Jul 12, 2011 at 4:15 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  We have to weld some supports (P°45) -  Fillet welds - in boilers tubes T91(PN 15E), T22 (PN°5A) and T12 (PN°4) grades, filler metal to be used is INCONEL.
Welders test is done GTAW/SMAW T12 Materials.
Accordind ASME, we have to qualify welders in this configuration but Client ask just to do one internal test, if visual is ok, welders can welds in production.

What we can do, as quality inspector, in this case?


Regards


--

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...