Mr. Fitria Rahman,

So far we are following SMAW+SAW with the following varaiable

First two pass with E7018 followed by SAW using the filler EM12K after the completion of one side, back grinding then SAW using the filler EM12K  ,we are getting good quality weld by this procedure, but the cost and time is seems to be very high .Can we avoid back welding by using the electrodes with good penetration like E7010 ?  Is it have any further alternatives available for us..?

Regards

Rinshad A


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...