     as per the code/specifications,, when welding starts we have to complete atleast 70% of the weld,if we stop welding due to some reasons u want to preheat the joint before the welding starts.

On Sat, Jul 16, 2011 at 6:23 PM, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:
Jagdish,

Making the root weld half done is not a good workmanship.

Also, most codes put a restriction for such things and at least root and hot pass must be completed before any interruption in welding.

What is your application of welding and check with your client spec.

Nandeesh




--- On Sat, 16/7/11, jagdish patil <jagdishpatil568@gmail.com> wrote:

From: jagdish patil <jagdishpatil568@gmail.com>
Subject: [MW:11747] weld stop during root pas
To: materials-welding@googlegroups.com
Date: Saturday, 16 July, 2011, 6:29 AM

Dear all,

 I would like to know during welding at root pass stage we stop some reason, but  we can start continue welding on next day without any test is it possible.
if not possible give me the specific reason.


regards,
JAGDISH

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...