On Tue, Jul 12, 2011 at 1:05 PM, JOSE SEBASTIAN <joseseban@gmail.com> wrote:
Dear Friends,
We have a qualified PQR for WB-36 Material using E 9018-G material and
we are using it in site.Now a vendor is supplying us 10018-G which is
more available.
Can I use 10018-G instead of 9018-G without qualifying PQR.I think in
both cases essential varialbles are same....
Also Is there any problem in using 9018-G instead of 10018-G without
qualifying PQR....
Regards,
Jose
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment