Dear Nagarajan,
Thank you for the information and the the time you had taken to review my query.However, I couldn't find A No.5.11 for the corresponding electrode in ASME BPV SEC IX.I think A No:5.11 would be SFA No. of electrode and typing error might have caused the problem.Please correct me,if I am wrong.
Regards,
Limesh
On Mon, Jul 11, 2011 at 6:08 PM, nagarajan uthanmalliah <unaga_1980@yahoo.co.in> wrote:
Dear Limesh,PNO:-11A,ASTM A553 Gr 1Filler Metal Class :-ERiCrFe-9F NO:43,A NO;5.11ThanksRegardsUthanmalliah Nagarajan
From: limesh M <limesh78@gmail.com>
Subject: [MW:11666] LNG Tank Material selection
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Monday, 11 July, 2011, 2:40 PM
Dear All,
What is the material normally used for LNG(Liquefied Natural Gas) tank fabrication?
I got some information that 9%Ni steel is OK(Still,I am not sure the authenticity of this information).
Apart from 9%Ni,any other material suitable for cryogenic application?
Actually what is this 9%Ni steel?
What is the correct designation of this 9%Ni steel in ASTM?
Regards,
Limesh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment