RE: [MW:11708] P1+P4 Fiiler

The higher grade base material may require the PWHT, not the consumable.  Remember, the PWHT may mitigate the microstructure of the base material HAZ,  What does your WPS require when joining the dissimilar materials?


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Naresh Kumar
Sent: Tuesday, July 12, 2011 3:49 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11702] P1+P4 Fiiler

Dear friends,

Thanks for your immediate response, But our client finally decided ER70S2+E 7018 instead

of  ER80S-B2+E 8018-B2; Also same as SA210 C+SA213 T11.Is that any specific reason???

Regards,

S.Nareshkumar



From: "Morin, Darcy (Bantrel Management Services)" <MorinD@BantrelManagementServices.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Mon, July 11, 2011 4:46:04 PM
Subject: RE: [MW:11680] P1+P4 Fiiler


 

 
API 582  has a useful chart for determining the filler metal for the joining of dissimilar steels.  Be sure to apply the appropriate PWHT.
 
 
 
Regards,
 
Darcy Morin


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Suresh
Sent: Monday, July 11, 2011 5:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11671] P1+P4 Fiiler

Dear Naresh ,
 
With reference to your question , go for ER 80S electrode ..which has being commonly used for both .
 
Thank you
 
Suresh

On Mon, Jul 11, 2011 at 2:03 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
Dear friends,

I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;

Regards,
S.Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This e-mail and any attachments may contain confidential and
privileged information. If you are not the intended recipient,
please notify the sender immediately by return e-mail, delete
this e-mail and destroy any copies.

Any dissemination or use of this information by a person other
than the intended recipient is unauthorized and may be illegal.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...