Dear friends,

 

Thanks for your immediate response, But our client finally decided ER70S2+E 7018 instead

of  ER80S-B2+E 8018-B2; Also same as SA210 C+SA213 T11.Is that any specific reason???

 

Regards,

S.Nareshkumar



From: "Morin, Darcy (Bantrel Management Services)" <MorinD@BantrelManagementServices.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Mon, July 11, 2011 4:46:04 PM
Subject: RE: [MW:11680] P1+P4 Fiiler


 

 
API 582  has a useful chart for determining the filler metal for the joining of dissimilar steels.  Be sure to apply the appropriate PWHT.
 
 
 
Regards,
 
Darcy Morin


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Suresh
Sent: Monday, July 11, 2011 5:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11671] P1+P4 Fiiler

Dear Naresh ,
 
With reference to your question , go for ER 80S electrode ..which has being commonly used for both .
 
Thank you
 
Suresh

On Mon, Jul 11, 2011 at 2:03 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
Dear friends,

I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;

Regards,
S.Naresh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

This e-mail and any attachments may contain confidential and
privileged information. If you are not the intended recipient,
please notify the sender immediately by return e-mail, delete
this e-mail and destroy any copies.

Any dissemination or use of this information by a person other
than the intended recipient is unauthorized and may be illegal.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...