Hi
Please see ASME Sec. VIII-Dev.1 ( 2010) UG-84 (i)
Best Regards
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Karthik
Sent: Tuesday, July 12, 2011 9:37 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11691] RE: 11664] Production impact test
Hi, Please refer UG 84(i)2 of ASME Section VIII div.1. PTP - Production Test Plate Thanks & Regards, (Karthik) Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
Dear AVA, On Mon, Jul 11, 2011 at 5:08 PM, AVA <ava.ssg@gmail.com> wrote: According to asme code, PTP is required when Impact test is essential. Best Regards From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sanu Krishnan Dear experts, Is it Production imact test required for LTCS,upto -50degree C.Already PQR Test qualified in -50 degree C? SANU.K.NAIR QC INSPECTOR DAEWOO E & C ABUDHABI Ph: 0507464738 -- -- -- |
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment