API 582 has a useful chart for determining the filler metal for the joining of dissimilar steels. Be sure to apply the appropriate PWHT.
Regards,
Darcy Morin
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Suresh
Sent: Monday, July 11, 2011 5:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11671] P1+P4 Fiiler
Dear Naresh ,
With reference to your question , go for ER 80S electrode ..which has being commonly used for both .
Thank you
Suresh
On Mon, Jul 11, 2011 at 2:03 PM, Naresh Kumar <snareshkumar30@yahoo.com> wrote:
--Dear friends,I have a doubt about SA106 B+SA335 P11 disimilar welding;Which electrode is best?? whether ER70S2 OR ER80S-B2;Regards,S.Naresh
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & Best Regards,
Suresh
Mobile No: 91-92 92 905 905
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment