Saturday, July 9, 2011

RE: [MW:11643] CLAD MATERIALS - WELD -PWHT

Thanks Manpreet Singh,

 

Yes, My case is option 2. I have received the Cladded material from Owner and need to perform only BUTT welding. (Weld overlay is not my case).

 

From your answer, I understood that I need to follow the PWHT Sec VIII 1, UCS -56, but what about the Clad material property during the PWHT. ( Any corrosion impact on the Clad portion).

 

Just I have only this doubt, Clad portion will withstand the ASTM G48 test after the PWHT.

 

With Kind Regards,                                      

 

S.Elumalai.


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of manpreet
Sent: Friday, July 08, 2011 2:29 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11635] CLAD MATERIALS - WELD -PWHT

 

Hi Sundaram,

 

Trust me, this can't be explained in single mail as you are not very specific with your question.

 

I assume procedure has to be qualified with ASME sec ix as Cladding has to be carried out for API pipes.

Process:- Try Pulse GMAW, can change deposition rates significantly

 

Refer AWS A5.14 for electrode

 

To qualify a procedure for corrosion resistant weld overlay, the welder must deposit a minimum 1.5" wide X 6" long pad of weld overlay on a test coupon using the guidelines/notes in QW-453. For performance testing, the welder must deposit a minimum 1/2" wide weld overlay consisting of a minimum of 3 weld beads in the first layer. This is done to achieve the necessary dilution with the base metal. There is no limit on the maximum number of layers for the weld overlay.

Base material, Consumable (AWS classification) and position should be within the allowable limits since these are essential variables, no limit on max thk of overlay deposit. 

PWHT is not applicable if you overlaying on the pipe but if you are butt welding 2 claddel pipes with inconel, it might be applicable to PWHT considering range of thickness per Sec Viii div 1 UCS-56 (i guess you are not going with 2nd option)

 

All tests per ASME Sec ix and Client spec:-

 

Dimensional Verification, visual inspection, Dye penetrant testing per Sec viii  div 1- App 8, dilution on weld surface shall not exceed 10% of base metal, root bead chemical analysis to match Inconel composition, transverse weld hardness survey (max 35 HRC), corrosion test (sour service), micrographic (*400)- microstructure of the HAZ should be free of precipitations and intermetallic phases, Side bends

 

For volumetric examination of CRA production groove welds, radiography (RT) is generally the best choice. Ultrasonic examination (UT) of CRA production groove welds is generally ineffective because of the nature of CRA weld metal 

 

Heat affected thickness to be minimized by lower heat input and higher travel speed.

 

Account all the suggestions and let us know ur case specifically.

 

 

Regards

Manpreet Singh



From: "Sundaram Elumalai"Elumalai.Sundaram@starfab.com.sa
Sent: Thu, 07 Jul 2011 18:25:41 +0530
To: materials-welding@googlegroups.com
Subject: [MW:11607] CLAD MATERIALS - WELD -PWHT

Hi Experts,

If anyone is having experience with the following CLAD materials, please give your input during the PQR / production weld. Is the PWHT will impact the corrosion property of Clad.

Pipe

NPS:10-Thk:45mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:15.88mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:45.5mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

Pipe

NPS:12-Thk:53.5mm-PIPE-API 5L GR.X65 PSL2 - SMLS -GA-E-61036

BW

3mm Inconel Cladded

With Kind Regards,

S.Elumalai.

******************************************************************************************
>CONFIDENTIALITY NOTICE
>This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.
>

--
>To post to this group, send email to materials-welding@googlegroups.com
>To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

******************************************************************************************
CONFIDENTIALITY NOTICE
This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

No comments: