Prem, thanks, In ASS preheating is done only in the early morning hours to drive away moisture or during damp weather. It has nothing to do with general preheating purpose for better weld making so to say.

--- On Fri, 8/7/11, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:

From: prem nautiyal <prem_nautiyal26@yahoo.com>
Subject: Re: [MW:11629] preheating of austenitic ss
To: materials-welding@googlegroups.com
Date: Friday, 8 July, 2011, 3:34 PM

Hi
 
Due to following three main reasons Austenitic Stainless Steel(ASS) are not preheated:
 
1. ASS have a very low Thermal conductivity, thus will retain heat for more time and will lead to more distortion
 
2. ASS have a very high thermal coefficient of expansion. If preheated will result in more distortion
 
3. Preheating will result in a wider HAZ and deteriorate the properties.
 
Regards
 
Prem S Nautiyal

--- On Fri, 7/8/11, khatri ankit <nids01dme011@gmail.com> wrote:

From: khatri ankit <nids01dme011@gmail.com>
Subject: [MW:11627] preheating of austenitic ss
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Friday, July 8, 2011, 1:58 PM

Dear Experts,

i want to know the technical reason that "why preheat is not required
in Austenitic SS"

what will the effects of that?

plz clarify me the reason.

Thanks and regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...