Friday, July 8, 2011

Re: [MW:11634] How can identify rolling direction in plate?

Dear Mr.Limesh..
 
You cann't identify the rolling direction in offcut plates or cut pieces..
 
msms

On Fri, Jul 8, 2011 at 9:27 AM, limesh M <limesh78@gmail.com> wrote:
Dear All,

For preparing test pieces for PQR, the following item to be fulfilled as per a document.

"For butt weld test assemblies Identification of the rolling direction of the used plates shall be provided."

My query is that,is it possible to identify the rolling direction by naked eye?If possible what is the trick behind it?



Regards,

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...