Wednesday, July 6, 2011

Re: [MW:11599] PRODUCTION WELDING WITH 2 WPS TO COVER THICKNESS RANGE AS PER BSEN

Hi,
As per EN you cannot combine the WPS

Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 7/6/11, manoj john <manojacgnr@gmail.com> wrote:

From: manoj john <manojacgnr@gmail.com>
Subject: [MW:11597] PRODUCTION WELDING WITH 2 WPS TO COVER THICKNESS RANGE AS PER BSEN
To: materials-welding@googlegroups.com
Date: Wednesday, July 6, 2011, 1:02 AM

 Dear All members,
 
I have 2 qualified procedures in SMAW process as per BSEN one procedure qulify a range of thickness 24mm maximum with single bevel and another procedure qualified a range of 25mm to 100 mm with double bevel.
 
My doubt is whether i can weld 50 mm thk plate with single bevel using with these 2 WPS. 
 
Thank you,
With best Reagards.
 
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...