Re: [MW:11575] A 106 Gr B 2" Pipes IMPACT TEST

dear sir,

the impact test is generally based on your mean time working temperature means the temperature at which your properties of the pipes & joint will be the resrained at subzero temp.

is it LPG LINE.

Regards

dinesh

On Fri, Jul 1, 2011 at 5:32 PM, lassaad mokrani <lassaad.mokrani@gmail.com> wrote:
Dear Experts,
Is impact test required by ASME (in PQR) or only by service conditions for 2" A106 Gr B pipe works???

Best Regards,
--
Meilleures salutations

Mokrani Lassaad
00216 20 649 755
http://www.linkedin.com/pub/lassaad-mokrani/16/364/907


















P     Pensez environnement! N'imprimez ce mail que si c'est vraiment nécessaire
Please consider your environmental responsibility before printing this e-mail


This e-mail is confidential and it is intended only for the addressees. Any
review, dissemination, distribution, or copying of this message by persons
or entities other than the intended recipient is prohibited. If you have
received this e-mail in error, kindly notify us immediately by telephone or
e-mail and delete the message from your system. The sender does not accept
liability for any errors or omissions in the contents of this message which
may arise as a result of the e-mail transmission

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35614] Re: SS FILLER

dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...