[MW:11781] PWHT and NDT requirement for SPENT CAUSTIC LINES

Dear Experts,
 
We have 2" sch 160 &  4" sch 80  C/S Piping welding ,whether  we need to conduct PWHT  for these lines or no need ,  because as per standard  CAUSTIC service lines need PWHT. but in our package the service fluid is SPENT CAUSTIC  and I want to know what is the required  percentage of NDT  for these service lines,

Please send suggestion & if any specific documents..

Thank you,
MPK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step