Hi Experts,

Could anybody tell maximum Hardness value for the following materials with code reference .What is the effect of heating by flame torch on these material ,( Flame heating is done to remove chocked polymer from inside the pipe by contractor )

1.ASTM A 106 GR.B, A105, A 234 ( CS Pipe and Fittings ).

2.ASTM 516 GR.70 ( CS Plate )

3.ASTM A 312 TP 304, 304L.316, -A182 TP 304,304L,316.- A403 ( SS Pipe and Fittings )

PWHT is not applicable as per code and service  and NACE is not applicable not for sour service .

Construction code: ASME B 31.3 and ASME Sec VIII Div I

Welding : ASME Sec IX.

Waiting for your detailed reply.

Regards,

SAIFULLA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...