Hello Experts,

Is production test is required as per B31.3 for,
Material: A333 GR6 LTCS PIPE
WPS USED: QUALIFIED AT -50 DEGREE CELCIUS.
CLIENT REQUIREMENT: AS PER B31.3.
--