hi ,
For the rolling direction of the plates i would look at the edges
of the plates mostly the sheared edges and the original untouched
edges could help to identify .
Also i would say that along the length of the plate would be the
rolling direction in majority of the cases...
This would e applicable only for full sized plates...
hope this will help
regards
hepo

On Jul 8, 9:42 am, Nandesh Kumar <nandeshku...@rocketmail.com> wrote:
> Limesh,
>  
> Normally the direction in which the data is stenciled/printed/painted will be the direction of rolling.
>
> Regards,
> Nandeesh
> --- On Fri, 8/7/11, limesh M <limes...@gmail.com> wrote:
>
> From: limesh M <limes...@gmail.com>
> Subject: [MW:11619] How can identify rolling direction in plate?
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Friday, 8 July, 2011, 3:57 AM
>
> Dear All,
>
> For preparing test pieces for PQR, the following item to be fulfilled as per a document.
>
> "For butt weld test assemblies Identification of the rolling direction of the used plates shall be provided."
>
> My query is that,is it possible to identify the rolling direction by naked eye?If possible what is the trick behind it?
>
> Regards,
>
> Limesh
>
> #yiv114967509 #yiv114967509avg_ls_inline_popup {padding:0px 0px;margin-left:0px;margin-top:0px;width:240px;overflow:hidden;word-wrap:br­eak-word;color:black;font-size:10px;text-align:left;line-height:13px;}
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...