[MW:11605] Re: tack weld of 1.4308 impeller and impeller wear

ER308/E308

On Jul 6, 1:13 pm, Ahmed Eissa <ahmedeiss...@yahoo.com> wrote:
> dear,
>  
> please what is the best electrode to be used to just perform tack weld of above mensioned material.
>  
>  
> thanks

--