[MW:11597] PRODUCTION WELDING WITH 2 WPS TO COVER THICKNESS RANGE AS PER BSEN

 Dear All members,
 
I have 2 qualified procedures in SMAW process as per BSEN one procedure qulify a range of thickness 24mm maximum with single bevel and another procedure qualified a range of 25mm to 100 mm with double bevel.
 
My doubt is whether i can weld 50 mm thk plate with single bevel using with these 2 WPS. 
 
Thank you,
With best Reagards.
 
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...