Sunday, July 3, 2011

[MW:11582] Re: A 106 Gr B 2" Pipes IMPACT TEST

It depends upon your service condition and MDMT, and customer
requirements.
If impact test is required on material you'll have to qualify PQR for
Impact test only.

You can use the same WPS to weld a test piece and test impact at
required tempreture and attached with your previous PQR as an
Addenda.

On Jul 1, 7:32 pm, lassaad mokrani <lassaad.mokr...@gmail.com> wrote:
> Dear Experts,
> Is impact test required by ASME (in PQR) or only by service conditions for
> 2" A106 Gr B pipe works???
>
> Best Regards,
> --
> Meilleures salutations
>
> Mokrani Lassaad
> 00216 20 649 755http://www.linkedin.com/pub/lassaad-mokrani/16/364/907
>
> P     Pensez environnement! N'imprimez ce mail que si c'est vraiment
> nécessaire
> Please consider your environmental responsibility before printing this
> e-mail
>
> This e-mail is confidential and it is intended only for the addressees. Any
> review, dissemination, distribution, or copying of this message by persons
> or entities other than the intended recipient is prohibited. If you have
> received this e-mail in error, kindly notify us immediately by telephone or
> e-mail and delete the message from your system. The sender does not accept
> liability for any errors or omissions in the contents of this message which
> may arise as a result of the e-mail transmission

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...