Wednesday, May 18, 2011

Re: [MW:11084] Super duplex material

Dear Mr.Praneeth,
 
You can use this filler wire for Super Duplex Material. but what is the UNS number 32750 or 32760????.
Somany brands are available in Market..Can you please tell me what are all the requirements for Testing???
Testing means CPT temp and method, Impact, Chemical, Mettalurgical, Micro Examination, intermettalic phase requirements...!!!
 
Important Note: Please ask the fillerwire manufacture about your requirements before the selection of Brand...!!!
 
SDSS is not a Normal One to get the positive results EASY, Especially CPT..!!!!
 
Regards
Ramkumar.J

On Tue, May 17, 2011 at 5:54 PM, praneet varma <praneethm14@gmail.com> wrote:
Dear experts,
Can we use Blue max- (LNT 100 X ) Filler wire in 6G position, for Super duplex materials.
 
Please clarify.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...