Re: [MW:11046] PQR with Impact test, Thick Qualified

Sorry See QW-451.1 for non impact test

2011/5/13 Salomo Ginting <omogin@gmail.com>
See QW-403.6


2011/5/11 Zakaria ghrab <zakaria.ghrab@gmail.com>
Hi all,

  I have one PQR 9 mm thick, with impact test. The range qualification of qualified WPS with Impact test is 9 mm to 16 mm according QW 403.6 .
My question is; What's the thick range qualification qualified by this PQR without impact test, where it's mention in ASME sect IX ?

Regards

--
زكرياء غراب
GHRAB Zakaria
مسؤول عن الجودة
QA/QC SENAD
مشروع المحطة الحرارية ـ الوحدة الرابعة
المحمدية ـ المغرب

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...