[MW:11045] RE: 11038] pup piece in every 1 km

Dear all,

 

6mtr is the minimum length requirement for the pup piece,

 

But using 6 mtr pup piece in every 1 KM of pipe line is not a requirement (or mandatory), and any client will not recommend also ( As per my previous experience)

 

Request you verify / provide the spec of the client if available.

 

 

 

Thanks & Regards

 

Lakshman kumar.B | Manager - QA/QC | LANCO  INFRATECH LIMITED
Plot# 1255 | Sanjeevani Chowk | Mahanadi Vihar | Cuttack 753004

Phone : + 91-671-2445033| Mobile: +91 9937286851 | www.lancogroup.com

Go Green |The future will thank you: Lakshman.kumar@lancogroup.com, Lakshmankumar4@gmail.com

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of limesh M
Sent: Thursday, May 12, 2011 12:33 PM
To: Materials & Welding
Subject: [MW:11038] pup piece in every 1 km

 

Dear All,

 

Why some client specification requires 6 m pipe pup piece in every 1 km pipeline?

 

Regards,

 

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...