Wednesday, May 18, 2011

[MW:11080] SA-213 Gr.T91

Dear Experts
 
What's the P.No. of Material Specification of SA-213 Gr.T91?
 
I refer Sec.IX 2010 Edition as per QW-422 - it's P.No.5B Gr.No.2
                                         as per Appendices-D - it's mentioned P.No.15E Gr.No.1
 
Which one is the correct?      

 
 
With Regards
 
 
Srinivasu V
Welding Engineer

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...