Thursday, May 5, 2011

[MW:10953] Reg:welder qualification

dear experts,

we have dissimilar materials  (only fillet weld is coming) between P9 to P8,due to lack of material we want to conduct welder test on production joint it self.we have welders qualified in P9 (FNo.6) and P8 (FNo6),
but for now we are using filler wire ERNiCr-3 (F.No43) for dissimilar materials.how we can qualify welder on fillet weld.is there any applicable standard is there?pl let me know.

thanks & regards


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...