Thursday, July 22, 2010

RE: [MW:6087] Distance education for Welding Engineeing

Hai,

 

Pl.  check  the web site: www.iiwindia.com  ------AMIIW-Exam(B. Tech-welding  Technology, Which is  approved  by Ministry  of  HRD-Govt. of  India).

 

I am also studying  the  same.

 

Any  help   contact  me  …

 

 

Thanks,

Regards,

 K.NANDAGOPAL ;

+91 9698997022

+91 9360049258-

Tamilnadu,

INDIA

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sayee
Sent: Wednesday, July 21, 2010 12:13 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:6048] Distance education for Welding Engineeing

 

Cranfield university runs a distance education MSc in welding engineering. The OU also runs a programme, which gives you credit towards IWE/ EWE. if interested I can post details including contacts with both programmes.

Kindest regards

Sayee Raghunathan

 

Mobile: 07500010806

 

Sent using my handheld

 

 


On 21 Jul 2010, at 07:33, "Bathula Raghuram (Mumbai - PIPING)" <R.Bathula@ticb.com> wrote:

IIW conducts AMIIW examination (equivalent to bachelors degree in welding engineering), check @ www.iiwindia.com


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim PK
Sent: Wednesday, July 21, 2010 11:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:6042] Distance education for Welding Engineeing

Hi,

 

Is there any distance education courses for Welding Engineering Diploma/Degree in India?

If available please share the details.


Thanks & Regards
Muhammed Ibrahim PK


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...