Friday, July 23, 2010

[MW:6093] Flux to be used in SAW with PWHT

Dear all,
My vendor is using WPS as follows:
Process - FCAW + SAW
Base Metal - S355 K2G3/ API 2H /2W GR 50
Thickness - 50 mm & above
Wire for FCAW - E71T-1
Wire for SAW - EH 12K & Flux - F 7A8
Preheat Temp.- 100 to 125 deg.C
PWHT  Temp. - 500 to 520 deg.C
As per
ASME Sec - II C Flux to be used shall be F 7P8 ( A denotes- as weld conditions &
P denotes for PWHT)                           
As  WPS includes PWHT Flux shall be used F 7P8.
Pl. guide me, weather flux used by the vendor is acceptable & if not what is to be done for the weld joints,those have been welded till date.  
Pl. reply urgently.
PSP


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...