Thursday, July 22, 2010

[MW:6079] Welding of ASTM A 335Gr.P11

Can we use E-7018B2 instead of E-8018B2 for welding of A-335 Gr. P11
material. If yes then what care shall be exercised during welding?
Would the resulting weldment be of adequate strength?


Thanks and Regards

Limesh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...