Wednesday, June 3, 2009

[MW:2316] UT welding query

Dear friends,
1) Is anybody will help me in finding the method of testing Ultrasonic testing of Fillet weld in 2inch plates of En-9.
2) Is there any method to detect vertical hair line crack in the butt welding 1inch ( 25mm) plates.

Regards,
Puneet


Own a website.Get an unlimited package.Pay next to nothing.*Go to http://in.business.yahoo.com/


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...