On Mon, Nov 24, 2008 at 6:01 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
members are requested to post with appropriate subject line which are relavnt the group motto, and as many details as possible.

Note: a request to all new members - please go thro the message thread titled "How to ask (or post a query) and get a quick and effective reply from the members of this forum!"

Thanking you for co opeartion


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...