Tuesday, June 2, 2009

[MW:2298] Cr. cabide exothemic in SS cladding

When you need TIG clad welding on A387-11-2 with ER309L rod and PWHT
is requird after welding in 690 dgree (for service resons),fracture
happend in bend test.becuse the Cr. cabide exothemic.
In this case how can slove this problem?

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...