i)                    We require to have restoration/ overlay of Monel (NiCu7)cladding by SMAW,GTAW, process ,where Specification restricts for Max Fe 2.5% for top 3mm of monel (NiCu7)weld overlay (We require  to weld overlay on SA 516Gr 70 and P4 material having thk of 10mm min)

ii)                   Will you please guide

a)      Which is the best consumables  brand to achieve Fe 2.5% max for top 3mm weld overlay?

b)      What is the min overlay height possible to achieve above requirement.?

c)       In case of monel clad restoration , generally we get the clad of 4mmthk

d)      What is the best welding parameter ?

e)      Due to cost implication ,we want to achieve the required chemistry of NiCu7 with max 2.5% Fe  at optimum overlay height say 5 to 6mm

 

 

Warm regards

 

Hegde P.B.

DGM (Welding Technology)

ISGEC Dahej

Gujarat India

+919714714803

 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...